Abstract
It was shown that immersing 25-mm thick rubber [Hevea brasiliensis] wood in a 10 boric acid equivalent solution containing 0. 5 Na-PCP for 40 min gave adequate loading of chemicals even at ambient temp. of about 30 deg C. Increasing the immersion time did not increase the loading appreciably